Under extrusion can have some different causes. A clogged nozzle, slipping extruder gear, the wrong filament diameter / extrusion multiplier settings in your slicer program.

A cold pull works best with slippery, soft materials – like Nylon filament.

Again, heat up your hotend to the working temperature of your Nylon or Polyamide filament, push it through the hotend as far as possible, ideally, until your previous material is cleaned out, which obviously is going to be somewhat hard if your nozzle is completely clogged. Then have the hotend cool down.
What we recommend is to set the hotend to 110, 120°C and just keep on pulling on the filament while the hotend is heating until the filament plops out in one piece. Then cut off the impure end of the filament, fully heat the hotend again and repeat the process until the pulled end of your filament comes out clean and you’ve restored good flow through the nozzle. Usually, two or three passes should be enough.

Tools needed:

Nylon Filament about 1m (about 3 feet)

Cleaningfilament

7,90

50g | Cleaningfilament gegen verstopfte 3D Drucker Düsen.

  • 1,75mm
  • 2,85mm
Auswahl zurücksetzen
Artikelnummer: n.a. Kategorie:

Beschreibung

Es kann passieren das die Düse eines 3D Druckers verstopft. Mit dem Cleaningfilament auf Nylon basis lässt sich dieses Problem ganz einfach lösen. Dieses Filament basiert auf der gleichen hochwertigen Formulatur die in allen PrintaMent Filamenten zum Einsatz kommt.

Zusätzliche Information

Durchmesser

1,75mm, 2,85mm

Menü